Din avgränsning ger 374 träffar.
-
2011:26 The influence of temperature and fluid pressure on the fracture network evolution around deposition holes of a KBS-3V concept at Forsmark, Sweden
In preparation for the review of SKB’s license application for disposal of spent nuclear fuel, SSM is conducting studies to evaluate the performance of the multi-barrier principle on which the KBS-3 concept is based. Copper canisters containing the spent nuclear fuel are placed into granitic bedrock at about 500 m depth and embedded in clay. Thus, the rock, the clay and the copper canister...
Innehållstyp: Publikationer -
2012:11 Issues in the corrosion of copper in a Swedish high level nuclear waste repository
The objective with this research project was to increase knowledge in the area of copper corrosion in the planned repository environment and obtain information on how copper corrosion evolves during the assessment period of 100 000 years. The equilibrium chemical composition of groundwater close to the canister as a function of temperature has been calculated by use of a thermodynamics code...
Innehållstyp: Publikationer -
2012:08 Deterministic Assessment of Future Costs for Dismantling (FA)
In this study a model for advanced deterministic cost calculation has been used to find a parametric value on the cost for dismantling of the FA-facility. The study gives good description of good practise to collect, test and utilise input data in a systematic way in order to make prudent cost estimates for any particular nuclear installation The Swedish Law stipulates that future expenses...
Innehållstyp: Publikationer -
2012:15 Technical Note, A review of the mechanical integrity of the canister
An introductory review of SR-Site has been conducted with respect to the mechanical integrity of the canister. The review is focused on the copper canister and the nodular cast iron insert. Review results show that a number of loads and loading scenarios for the copper canister has not been analysed by SKB. The importance of sufficient creep ductility of the copper material and sufficient...
Innehållstyp: Publikationer -
2012:30 Technical Note, Initial review of physical properties and processes of the buffer and backfill. THM and other physical processes
The Swedish Radiation Safety Authority (SSM) reviews the Swedish Nuclear Fuel Company’s (SKB) applications under the Act on Nuclear Activities (SFS 1984:3) for the construction and operation of a repository for spent nuclear fuel and for an encapsulation facility. As part of the review, SSM commissions consultants to carry out work in order to obtain information on specific issues. The...
Innehållstyp: Publikationer -
2012:25 Workshop on Seismology
This report summarizes the issues discussed at the workshop and extracts the essential viewpoints that have been expressed. The report is not to consider as a comprehensive record of all the discussions at the workshop and individual statements made by workshop participants should be regarded as opinions rather than proven facts. This report includes, apart from the workshop synthesis, the...
Innehållstyp: Publikationer -
2012:28 Technical Note, Initial review of chemical and erosional processes within the buffer and backfill – Geochemical processes
This report consists of a Technical Note in SSM’s initial review phase of SKB’s safety analysis SR-Site. The aim of the initial review of issues concerning geochemical processes in buffer and backfill in a final repository is to make a broad illustration and review of SR-Site together with its subordinate references, as well as to identify potential needs for complementary information or...
Innehållstyp: Publikationer -
2017:18 FEM analysis of the mechanical integrity for the canister intended for storage of spent nuclear fuel with regard to copper creep ductility
Background For final storage of spent nuclear fuel it is suggested by the Swedish nuclear fuel and waste management company (SKB) to emplace the nuclear fuel into copper canisters which are surrounded by bentonite clay at approximately 500 meters’ depth into granitic rock. After emplacement of the canisters Bentonite swelling due to water saturation and hydrostatic pressure build up the...
Innehållstyp: Publikationer -
2017:28 SSM’s external experts’ review of SKB’s safety assessment SR-PSU - hydrogeology, geochemistry and bentonite
Main review phase...
Innehållstyp: Publikationer -
2009:30 A Review of Evidence for Corrosion of Copper by water
The planned spent nuclear fuel repository in Sweden relies on a copper cast iron canister as the primary engineered barrier. The corrosion behaviour of copper in the expected environment needs to be thoroughly understood as a basis for the post-closure safety analysis. It has been shown that corrosion may indeed be the primary canister degradation process during the utilised assessment period...
Innehållstyp: Publikationer