Din avgränsning ger 1 träffar.
-
00:57 Application of the Pin-Loading Tension Test to Measurements of Delayed Hydride Cracking Velocity in Zircaloy Cladding
2337 kB ... C13(W=19) 13-1 13-2 13-3 Figure 2 Elastic compliance as a function of crack length a/W. APPENDIX C3(3) The trend for the experimental points, which are shown in Figure 2, is characterised by Equation...